6. Bearing strength and failure behavior of hybrid composite laminates.
University essay from Linköpings universitet/KonstruktionsmaterialAbstract : Composite layups have been continuously used over many years in various applications. It is necessary to optimize its composition by studying various parameters influencing the mechanical properties and studying the failure behavior. READ MORE
-
7. Effects of Austempering Process on Mechanical Behavior Properties of Compacted Graphite Iron
University essay from Högskolan i Jönköping/JTH, Material och tillverkning; Högskolan i Jönköping/JTH, Industriell produktutveckling, produktion och designAbstract : The thesis paper here focuses on the effects of the austempering temperature (TA) and the austempering time (tA) on the unalloyed fully ferrite Compacted Graphite Iron (CGI), to obtain improve in mechanical properties and the study of the microstructure. The unalloyed CGI samples were austenitised at 850oC for 60 and 90 min and were then heat treated at 275, 325 and 375oC with different holding times at 30,60,90, and 120 mins. READ MORE
-
8. Fractography, mechanical and structural analysis of trabecular bone from the femoral head of human cadavers
University essay from Lunds universitet/Avdelningen för Biomedicinsk teknikAbstract : A lowered mineral density in the skeletal bones may indicate osteoporosis and an increased risk of fragility fractures. However, lower bone mass does not reveal the whole truth about the status of the bone quality. READ MORE
-
9. Hydrogen-assisted stress corrosion cracking of high strength steel
University essay from KTH/Skolan för kemivetenskap (CHE)Abstract : In this work, Slow Strain Rate Test (SSRT) testing, Light Optical Microscopy (LOM) and Scanning Electron Microscopy (SEM) were used to study the effect of micro-structure, corrosive environments and cathodic polarisation on stress corrosion cracking (SCC) of two grades of high strength steels, Type A and Type B. Type A is manufactured by quench and tempered (Q&T) method. READ MORE